Image of KEKUATAN TARIK DAN MORPOLOGI SERAT PELEPAH KELAPA DAN BATANG PISANG Nasmi Herlina Sari, Rakhmat Khaqiqi, Agus Dwi Chatur*

Tugas Akhir Mesin

KEKUATAN TARIK DAN MORPOLOGI SERAT PELEPAH KELAPA DAN BATANG PISANG Nasmi Herlina Sari, Rakhmat Khaqiqi, Agus Dwi Chatur*

Rakhmat Khaqiqi - Nama Orang;

Natural fibers are often considered as replacement fibers that are environmentally friendly compared to synthetic. applications from natural fibers develop in several sectors such as automotive, Furniture, packing and construction. The purpose of this study was to investigate the properties of the tensile strength and morphology of coconut bark fibers and banana stem fibers, which is treated alkaline Sodium Hydroxide (NaOH) and Potassium hydroxide (KOH). with a concentration of 8% each and soaked for 2 hours. the results of the study show that the highest tensile strength analysis on coconut midrib fiber used by 8% NaOH was 338.94 MPa, In SKNA, high tensile strength was obtained because it was influenced by SEM analysis on the coarser fiber surface and the wax layer was lost due to the alkali process. For coconut midrib fiber obtained the tensile strength value at SKTP of 148.57 Mpa, SKNA of 338.94 MPa, and SKKA of 74.67 MPa. Whereas for banana stem fibers shows the results of the highest tensile strength analysis of banana stem fibers which are treated with 8% KOH with a value of 894.91 MPa, in SPKA obtained high tensile strength because it is influenced by the results of SEM analysis on coarser fiber surfaces and wax and cellulose layers that have been lost due to the alkali process. For banana stem fibers obtained the value of tensile strength on SPTP of 691.14 MPa, SPNA of 585.82 MPa, and SPKA of 894.91 MPa. From the data obtained, the alkali treatment of coconut mindrid and banana stems effects tensile strength, functional groups, crystallinity indeks and morphology.


Ketersediaan
201809634.606.Rah.kPerpustakaan Fakultas TeknikTersedia
Informasi Detail
Judul Seri
-
No. Panggil
634.606.Rah.k
Penerbit
Universitas Mataram : Fakultas Teknik Unram., 2018
Deskripsi Fisik
x,56 Hlm, Illus, 21x29 cm
Bahasa
Indonesia
ISBN/ISSN
-
Klasifikasi
634.606
Tipe Isi
other
Tipe Media
other
Tipe Pembawa
-
Edisi
Edisi 1 Jilid 1
Subjek
SERAT PELEPAH KELAPA
Coconut Frounds Fiber, Banana
Strem Fiber, Tensile Strength, FT-IR, SEM, XRD
Info Detail Spesifik
-
Pernyataan Tanggungjawab
Rakhmat Khaqiqi
Versi lain/terkait

Tidak tersedia versi lain

Lampiran Berkas
  • KEKUATAN TARIK DAN MORPOLOGI SERAT PELEPAH KELAPA DAN BATANG PISANG Nasmi Herlina Sari, Rakhmat Khaqiqi, Agus Dwi Chatur*
Komentar

Anda harus login sebelum memberikan komentar

Perpustakaan Fakultas Teknik
  • Informasi
  • Layanan
  • Pustakawan
  • Area Anggota

Tentang Kami

Ruang Baca Fakultas Teknik

Kami menyedian Buku ajar ilmu teknik dan Tugas Akhir mahaiswa Fakultas Teknik Universitas Mataram

Cari

masukkan satu atau lebih kata kunci dari judul, pengarang, atau subjek

Donasi untuk SLiMS Kontribusi untuk SLiMS?

© 2025 — Senayan Developer Community

Ditenagai oleh SLiMS
Pilih subjek yang menarik bagi Anda
  • Karya Umum
  • Filsafat
  • Agama
  • Ilmu-ilmu Sosial
  • Bahasa
  • Ilmu-ilmu Murni
  • Ilmu-ilmu Terapan
  • Kesenian, Hiburan, dan Olahraga
  • Kesusastraan
  • Geografi dan Sejarah
Icons made by Freepik from www.flaticon.com
Pencarian Spesifik